LAISHA
Open Laisha

ICAR AICE-JRF/SRF Wood Anatomy & Wood Properties: practice questions

ICAR AICE-JRF/SRF (PhD) — Subject 59 Forestry · India · National Testing Agency for ICAR

Original practice questions written to the published syllabus · not past papers
10worked here, free
38written to this exam in this subject
11syllabus units

About ICAR AICE-JRF/SRF

ICAR AICE-JRF/SRF (PhD) — Subject 59 Forestry is a PhD, fellowship and lectureship exam run by National Testing Agency for ICAR, for candidates in India. Computer-based, 2 hours, 120 MCQs (Part A 20 general; Part B 50 core group; Part C 50 subject), +4 / −1, maximum 480.

Source: icar.org.in.

Checked against the exam body's published information. Formats and fees change; confirm the current edition there before you book.

Wood Anatomy & Wood Properties in ICAR AICE-JRF/SRF

MCQs on wood anatomy (softwood and hardwood structure, cell wall), wood properties and their relation to utilisation.

The structure of wood and how it determines strength, density, durability and use: macroscopic and microscopic identification of timbers and their physical and mechanical properties.

Our 38 ICAR AICE-JRF/SRF questions in this subject: 1 easy, 12 medium, 25 hard, across 11 units.

10 practice questions, worked

Choose an answer, then open the working. Each explanation says why the right answer is right and why the others are not.

These 10 were written to ICAR AICE-JRF/SRF and are not shown on any other exam's page.

Question 1 · hard

Why is sapwood of all species non-durable?

  1. It contains much more lignin than heartwood does
  2. It is always denser than heartwood
  3. It lacks extractives and holds starch and sugars
  4. It is formed only in winter
Answer and working

C. It lacks extractives and holds starch and sugars

Without protective extractives and with stored food, sapwood attracts fungi and insects.

Question 2 · hard

Juvenile wood near the pith typically has, compared with mature wood:

  1. Shorter cells, larger microfibril angle and lower density
  2. Longer cells, smaller microfibril angle and higher density
  3. No cell walls
  4. Identical properties in every species
Answer and working

A. Shorter cells, larger microfibril angle and lower density

Fast-grown plantations often contain much juvenile wood.

Question 3 · medium

Normal (constitutive) resin canals occur in:

  1. Firs, true cedars and hemlocks of temperate forests
  2. Pines, spruces, larches and Douglas-fir
  3. All hardwoods
  4. Teak and sal only
Answer and working

B. Pines, spruces, larches and Douglas-fir

Firs, cedars and hemlocks may form only traumatic canals after injury.

Question 4 · hard

Deodar (Cedrus deodara) normally:

  1. It may have large normal axial and radial resin canals like pines
  2. Lacks normal resin canals but can form traumatic ones
  3. Has vessels with simple perforations
  4. Has storied rays
Answer and working

B. Lacks normal resin canals but can form traumatic ones

Cedars form traumatic canals in tangential rows after injury.

Question 5 · hard

Fine ripple marks on tangential surfaces of Dalbergia and Pterocarpus result from:

  1. Storied structure of rays and other elements
  2. Spiral grain running around the stem
  3. Tyloses in vessels
  4. Compression wood
Answer and working

A. Storied structure of rays and other elements

Elements arranged in horizontal tiers produce ripple marks.

Question 6 · hard

The main determinant of density and strength in hardwoods is:

  1. Number of resin canals per square millimetre
  2. Width of the pith
  3. Proportion and wall thickness of fibres
  4. Colour of heartwood
Answer and working

C. Proportion and wall thickness of fibres

Thick-walled fibres provide most of the mass and support.

Question 7 · hard

DART-TOFMS identifies timber by its:

  1. Growth ring width
  2. Chemical profile
  3. Colour under sunlight
  4. Sound when struck
Answer and working

B. Chemical profile

Mass spectrometry detects characteristic compounds.

Question 8 · hard

A wood has total tangential shrinkage of 8% and FSP of 28%. Assuming linear shrinkage below FSP, what tangential shrinkage occurs on drying to 12% MC?

  1. 3.4%
  2. 4.6%
  3. 8.0%
  4. 12.0%
Answer and working

B. 4.6%

8 × (28 − 12)/28 = 4.6%. 3.4% uses 12/28 instead of (28 − 12)/28; 8% is shrinkage to oven-dry.

Question 9 · medium

A 20 × 20 mm clear specimen on a 300 mm span fails at a centre load of 2000 N. Using MOR = 3PL/(2bd²), what is its modulus of rupture?

  1. 75.0 N/mm²
  2. 112.5 N/mm²
  3. 225.0 N/mm²
  4. 56.3 N/mm²
Answer and working

B. 112.5 N/mm²

MOR = 3 × 2000 × 300/(2 × 20 × 400) = 112.5 N/mm². Omitting the 3 gives 75; omitting the 2 in the denominator gives 225.

Question 10 · hard

Brittleheart in large tropical logs is caused by:

  1. Fungal decay of the sapwood in standing trees
  2. Insects boring the pith
  3. Long-term compressive growth stress near the centre
  4. Fire scars
Answer and working

C. Long-term compressive growth stress near the centre

The central wood fails in compression over decades.

A study plan for Wood Anatomy & Wood Properties in ICAR AICE-JRF/SRF

This plan follows where our questions actually fall, so the time goes where the marks are likely to be. It is our reading of the syllabus, not the exam body's weighting.

  1. First, the heavy units (45% of the 38 questions): Mechanical properties: bending, compression, hardness (5, 13%); Cell wall structure and chemical composition (4, 11%); Hardwood structure: vessels, fibres, parenchyma; ring-porous and diffuse-porous (4, 11%); Wood-water relations: moisture content, fibre saturation point, shrinkage (4, 11%).

    Read the manual chapters for these first and do every worked question you can find on them.

  2. Then the middle band: Formation of wood: cambium, sapwood and heartwood (3, 8%); Macroscopic and microscopic identification of timbers (3, 8%); Natural defects and reaction wood (3, 8%); Natural durability of timbers (3, 8%).

    Aim for one sitting per unit, then mixed questions across them.

  3. Then the lighter units: Softwood structure: tracheids, rays, resin canals (3, 8%); Timber grading and the uses of important timbers (3, 8%); Wood density and specific gravity (3, 8%).

    Learn the definitions, classifications and standard numbers; these units are more often recalled than worked.

  4. Leave time for the hard ones: Hardwood structure: vessels, fibres, parenchyma; ring-porous and diffuse-porous (3 hard of 4), Wood-water relations: moisture content, fibre saturation point, shrinkage (3 hard of 4), Formation of wood: cambium, sapwood and heartwood (2 hard of 3).

    Come back to these after a first pass, untimed, and read every explanation, including for the options you rejected.

  5. Bank the easy marks: Cell wall structure and chemical composition (1 easy of 4).

    Do these early in revision so they are fast on the day.

  6. Finish timed. Sit the subject as a timed set without notes, mark it, and send each wrong answer back to its unit above.

Last updated · How Laisha writes and checks its pages · Report a mistake

Ask Laisha about this

Opens Laisha's chat with your question ready to send. Sign in or start free.

Unlock every question — ICAR AICE-JRF/SRF Wood Anatomy & Wood Properties

US$10 a month · one price worldwide · cancel any time

  • Every practice question in this subject, with full working
  • Timed exam papers and progress by unit
  • Ask Laisha to explain any answer — up to 1,000 questions a month
Free or Smarter
FreeSmarter
Grow guides, pest pages, articlesRead allRead all
Ask Laisha5 a dayUp to 1,000 a month
Exam practiceThe sample on each pageEvery question, timed papers
Crop calendar and pest alerts—For your own fields
Calculators and tools—All
Uploads and reports—100 a month, real files
10 days free for every new account, no card.